高溫合金上海鋼材免費(fèi)提供樣品化學(xué)成分: 碳C:≤0.08; 錳Mn:≤0.35; 硅Si:≤0.35; 磷P:≤0.015; 硫S:≤0.015; 鉻Cr:17.0~21.0; 鎳Ni:50.0~55.0; 鉬Mo:2.80~3.30; 鈮Nb:4.75~5.50; 鈦Ti:0.65~1.15; 鋁Al:0.20~0.80; 鈷Co:≤1.00; 磞B:≤0.006; 銅Cu:≤0.30; Mg:
高溫合金硬度檢測化學(xué)成分化學(xué)成分: 碳C:≤0.08; 錳Mn:≤0.35; 硅Si:≤0.35; 磷P:≤0.015; 硫S:≤0.015; 鉻Cr:17.0~21.0; 鎳Ni:50.0~55.0; 鉬Mo:2.80~3.30; 鈮Nb:4.75~5.50; 鈦Ti:0.65~1.15; 鋁Al:0.20~0.80; 鈷Co:≤1.00; 磞B:≤0.006; 銅Cu:≤0.30; Mg:≤0
高溫合金信譽(yù)保證正規(guī)貨源牌號:K441高溫合金 K441高溫合金化學(xué)成分 C(%): 0.11~0.18 Cr(%): 9.50~11.0 Mo(%): 3.50~4.20 Ni(%): 余量 Co(%): 9.50~10.5 W(%): 4.50~5.20 AI(%): 5.00~5.80 Nb(%): — Ti(%): 2.00~2.90 Fe(%): ≤0.5 Si(%)≤: 0.30
高溫合金鑄件鑄態(tài)供應(yīng) 化學(xué)成分Typical values(Weight %) Fe Mn Si P S Cu Pb Bi As Sn Sb ≤0.20 ≤0.20 ≤0.01 ≤0.0005 ≤0.01 ≤0.10 ≤0.001 ≤0.0001 ≤0.005 ≤0.002 ≤0.001 C Cr Co W Mo Al Ti Nb
高溫合金相對應(yīng)材質(zhì)的焊條化學(xué)成分: 碳C:≤0.08; 錳Mn:≤0.35; 硅Si:≤0.35; 磷P:≤0.015; 硫S:≤0.015; 鉻Cr:17.0~21.0; 鎳Ni:50.0~55.0; 鉬Mo:2.80~3.30; 鈮Nb:4.75~5.50; 鈦Ti:0.65~1.15; 鋁Al:0.20~0.80; 鈷Co:≤1.00; 磞B:≤0.006; 銅Cu:≤0.30; Mg:≤0